Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® EA513 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® WA550 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® WA551 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | |
Dow Questra® WA552 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm |
600 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP610 Paper Base Laminate Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm |
600 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Perpendicular in Oil; ASTM D149 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | |
Saint-Gobain CHR® SG03-05(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat St.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.17 mm |
600 kV/in @Thickness 0.125 in |
|
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of .. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | |
Cytec (Conap) FR-1080 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | ASTM D149 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Fluid Resistance |
3M TMW Tubing 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th.. |
|||
Dielectric Strength | >= 23.6 kV/mm | >= 600 kV/in | ASTM D149a |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | ASTM D149 |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Dielectric Strength | 23.6 kV/mm | 599 kV/in | ASTM D149 |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Average value: 23.6 kV/mm Grade Count:5 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Dielectric Strength | 23.6 kV/mm | 600 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |