Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ASTM D1457-18 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ASTM D792 |
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro.. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ASTM D792 |
P & P Technology EC-J Silver Aluminum Loaded Silicone P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties.. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ISO 1183 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ISO 1183 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ISO 1183 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ISO 1183 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Specific Gravity | 2.00 - 2.20 g/cc | 2.00 - 2.20 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Specific Gravity | 1.70 - 2.20 g/cc | 1.70 - 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Specific Gravity | 1.70 - 2.20 g/cc | 1.70 - 2.20 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6452 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Specific Gravity | 2.10 - 2.20 g/cc | 2.10 - 2.20 g/cc | ISO 1183 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D792 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D 792 |
Karina E 1000/HMB 21586 White Concentrate Color Concentrate Filled white concentrate designed for general purpose film applications based on olefin resins. Letdown ratio estimated from 1% to 5%.Information provided by Karina Indústria e Comércio de PlÃ.. |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | |
Garlock 8764 PTFE Rubber Sheet Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
Specific Gravity | 2.18 - 2.20 g/cc | 2.18 - 2.20 g/cc | ASTM D792 |
Adamas Adalon® 509 PTFE, 3% MoS2 Information provided by Adamas, HPM |
|||
Specific Gravity | 2.14 - 2.20 g/cc | 2.14 - 2.20 g/cc | ASTM D792 |
Technetics Group Texolon™ 8764 PTFE
(Unverified Data**) A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri.. |
|||
Specific Gravity | 2.12 - 2.20 g/cc | 2.12 - 2.20 g/cc | ASTM D792 |
Adamas Adalon® 911 PTFE Information provided by Adamas, HPM |