Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.14 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.14 g/cc
2.14 g/cc
Part A; TM R050-16
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
3M Dyneon™ FEP X 6301 UHP Fluorothermoplastic Fluorinated Ethylene Propylene  (discontinued **)
Dyneon FEP X 6301 UHP was designed primarily for ultra-high purity applications requiring very low levels of metals and ions. This extrusion grade of EEP is ideally suited for tubing, which can be u..
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
ASTM D792
Technetics Group Texolon™ 7865 PTFE  (Unverified Data**)
Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac..
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
ISO 12086
Isoflon PFA Polyperfluoroalkoxyethylene
Fluoropolymer material specifications.Information provided by Isoflon.
Specific Gravity 2.14 - 2.19 g/cc
2.14 - 2.19 g/cc
ASTM D792
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite
Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon.
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
ASTM D 792
Karina E 1000/HMB 21586 White Concentrate Color Concentrate
Filled white concentrate designed for general purpose film applications based on olefin resins. Letdown ratio estimated from 1% to 5%.Information provided by Karina Indústria e Comércio de PlÃ..
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
Garlock 8764 PTFE Rubber Sheet
Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc
2.14 g/cc
Part B
Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy
Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. ..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
A. Schulman POLYBATCH™ Popular Choice White HS80660 Concentrate Based In Polystyrene
DescriptionPOLYBATCH® HS80660 is a white masterbatch containing 70% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive..
Specific Gravity 2.14 g/cc

@Temperature 25.0 °C
2.14 g/cc

@Temperature 77.0 °F
Dow Corning SE 4446 CV KIT
Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility.Information provided by Dow Corning
Specific Gravity 2.14 - 2.16 g/cc
2.14 - 2.16 g/cc
ASTM D792
Adamas Adalon® 301 PTFE, 10% Graphite
Information provided by Adamas, HPM
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
ASTM D792
Adamas Adalon® 902 PTFE, 1% Conductive filler
Information provided by Adamas, HPM
Specific Gravity 2.14 - 2.18 g/cc
2.14 - 2.18 g/cc
ASTM D792
Adamas Adalon® 991 PTFE
Information provided by Adamas, HPM
Specific Gravity 2.14 - 2.18 g/cc
2.14 - 2.18 g/cc
ASTM D792
Adamas Adalon® 998 PTFE, Turquoise
Information provided by Adamas, HPM
Specific Gravity 2.14 g/cc
2.14 g/cc
ASTM D792
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules
Dyneon FEP 6301Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical ..
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
ASTM D792
Technetics Group Texolon™ 8764 PTFE  (Unverified Data**)
A premium PTFE sheet manufactured from the highest quality PTFE.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectri..
Specific Gravity 2.14 - 2.17 g/cc
2.14 - 2.17 g/cc
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff..
Specific Gravity 2.14 - 2.16 g/cc
2.14 - 2.16 g/cc
ASTM D792
Adamas Adalon® 305 PTFE, 15% Graphite
Information provided by Adamas, HPM