Material Notes:
High Density Hexene Copolymer Formolene® HP4306 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It is designed specifically for larger diameter and thick wall pipes where excellent melt strength is required, but can be used successfully on all diameters and wall thicknesses. It has good long-term hoop strength performance, very high melt strength, and outstanding toughness even at low temperatures. Formolene® HP 4306 meets all requirements of ASTM D4976 – PE 235. When blended with the approved color concentrates, Formolene® HP4306 has a cell class of 345464C per ASTM D3350-05, is listed by PPI as a PE3608 material with HDB's of 1,600 psi @ 73°F and 800 psi @ 140°F and meets the requirements of NSF Standard 14/61 for use with potable water. Formolene® HP4306 also qualifies as a PE3408 material under the old ASTM D3350-02a and PPI standards. Formolene® HP4306 also qualifies as a PE80 material per ISO 9080.Applications: Potable Water; Oil and Gas Gathering and Distribution; Chemical, Industrial and Mining; SewerInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Natural; ASTM D1505
0.955 g/cc
0.0345 lb/in³
Black; ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A, B, C, F<sub>50</sub>; ASTM D1693
Melt Flow 0.060 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.060 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
PENT 150 hour
150 hour
Slow Crack Growth; ASTM F1473
Tensile Strength at Break 34.5 MPa
5000 psi
2" (50mm) per min, Type IV; ASTM D638
Tensile Strength, Yield 22.1 MPa
3200 psi
2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 500 %
>= 500 %
2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
ASTM D3350
0.965 GPa
140 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746