Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dielectric conduits, antishock
Physical Properties Metric English Comments
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
ISO R 527
Tensile Strength, Yield 48.0 MPa
6960 psi
ISO R527
Elongation at Break 170 %
170 %
ISO R 527
Izod Impact, Unnotched 7.80 - 8.20 J/cm

@Temperature 23.0 °C
14.6 - 15.4 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 81.0 - 83.0 °C

@Load 5.00 kg
178 - 181 °F

@Load 11.0 lb
ISO R306