Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.80 - 8.20 J/cm @Temperature 23.0 °C |
14.6 - 15.4 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free Dielectric conduits, antishock |
|||
Izod Impact, Unnotched | 7.80 - 8.20 J/cm @Temperature 23.0 °C |
14.6 - 15.4 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free Electric antishock fittings |