Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare. |
|||
Izod Impact, Unnotched | 7.80 - 8.20 J/cm @Temperature 23.0 °C |
14.6 - 15.4 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free Dielectric conduits, antishock |
|||
Izod Impact, Unnotched | 7.80 - 8.20 J/cm @Temperature 23.0 °C |
14.6 - 15.4 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free Electric antishock fittings |