Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Extrusion Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be processed to 625°F and has excellent adhesive properties to substrates such as polypropylene, HDPE, PVdC, and paper.Applications: Seaming; Heavy duty shipping sacks; Dunnage bags; Tarpaulins; Agricultural and construction films; Pond liners; Medical packages. Data for film properties below based on 1.25 mil film.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
Exxon Method
Thickness 31.8 microns
1.25 mil
Melt Flow 6.0 g/10 min
6.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 290 %
290 %
ASTM D882
Film Elongation at Break, TD 620 %
620 %
ASTM D882
Secant Modulus, MD 0.120 GPa
17.4 ksi
ASTM D882
Secant Modulus, TD 0.140 GPa
20.3 ksi
ASTM D882
Coefficient of Friction 0.90
0.90
ASTM D1894
Elmendorf Tear Strength MD 100 g
100 g
ASTM D1922
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
Elmendorf Tear Strength, MD 3.15 g/micron
80.0 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 2.20 g/micron
56.0 g/mil
ASTM D1922
Dart Drop 3.15 g/micron
80.0 g/mil
F50; ASTM D1709
Dart Drop Test 100 g
0.221 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Film Tensile Strength at Break, TD 19.0 MPa
2760 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 102 °C
216 °F
Exxon Method
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 44 %
44 %
45°, ASTM D-2457
Users viewing this material also viewed the following: