Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | ASTM D882 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | ASTM D882 |
Eastman 5220 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good bubble stability, Medium coefficient of friction, Excellent low temperature properties, Good heat seal characteristicsApplica.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | ASTM D882 |
Eastman 5222 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good low temperature properties, Good heat seal characteristics, High slip, High antiblock, Good optical propertiesApplications:Ic.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | ASTM D882 |
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | ASTM D882 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |
|||
Secant Modulus, MD | 0.120 GPa | 17.4 ksi | 5%; ASTM D882 |
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |