Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® CP 1317 PRE-ELEC CP 1317 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1317 .. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® CP 1319 PRE-ELEC CP 1319 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1319 .. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1055 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms.. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1080 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under.. |
|||
Film Tensile Strength at Break, MD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |