Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 31.8 microns | 1.25 mil | |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2.2:1 BUR |
LyondellBasell Petrothene® NA334000 Low Density Polyethylene ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA340163 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Thickness | 31.8 microns | 1.25 mil | Cast, as tested |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA340013 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
Thickness | 31.8 microns | 1.25 mil | Cast, as tested |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake EF412 Low Density Polyethylene WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake EF421 Low Density Polyethylene WESTLAKE polyethylene EF421 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and general purpose food packaging app.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake Elevate™ EF437 2.5% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake Elevate™ EF561 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Thickness | 31.8 - 50.8 microns | 1.25 - 2.00 mil | Average value: 34.9 microns Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Thickness | 31.8 microns | 1.25 mil | side 2 layer 1; Arlon SQA-TMS-003 |
Arlon R37908R015L Silicone Rubber/Fiberglass/Acrylic/Polyester Laminated film: aluminized PEN; Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2, layer 1: acrylic PSA; Side 2, layer 2: polyester substrate; Side 2, layer 3: acrylic PSA; Interleav.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
M. Holland Company MAGMA® LL1092-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |