Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
LyondellBasell Petrothene® NA952000 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
LyondellBasell Petrothene® NA952094 Low Density Polyethylene
ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil LD 103.59 Industrial Film Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
Elmendorf Tear Strength TD 70 g
70 g
ASTM D1922
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..