Material Notes:
Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging.Availability: Latin America, North America and South America Applications: Closures and DispensersHousewaresProtective Caps Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 330 hour
330 hour
Condition B, 10%; ASTM D1693
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.72 MPa
1700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.4275 GPa
62.00 ksi
2% secant; ASTM D790
Flexural Modulus, 1% Secant 483 MPa
70000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 124 °C
255 °F
ASTM D3418
Vicat Softening Point 92.2 °C
198 °F
ASTM D1525
Descriptive Properties Value Comments
Features Standard processing antioxidants
Form PELLET