Material Notes:
Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hr; ASTM D570
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D635
Flexural Yield Strength 39.3 MPa
5700 psi
ASTM D790
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
0.5 inch; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in