All information provided by Hongkun Group
Physical Properties Metric English Comments
pH 1.2 - 2.2
1.2 - 2.2
Evaporation Loss <= 3.0 %
<= 3.0 %
loss on drying
Thermal Properties Metric English Comments
Melting Point >= 140 °C
>= 284 °F
Component Elements Properties Metric English Comments
Lead, Pb 0.00050 %
0.00050 %
heavy metal
Descriptive Properties Value Comments
Appearance off-white to light yellow powder
Cloudiness (EBC) <= 1.5
Color, APHA <= 1
Purity (%) >= 99.0