Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LL 1001x26 Blown Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 1001x26 Blown Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: YesThermal Stabilizer: YesApplications: Agricultural FilmBag in BoxBarrier Food PackagingBlown FilmBread BagsFood packagingForm Fill and Seal PackagingFreezer FilmGarment FilmGeneral PackagingHeavy Duty BagsIce BagsIndustrial LinersIndustrial PackagingLamination FilmLinersMultilayer Packaging FilmPackaging FilmsProduce BagsRefuse BagsShoppersStand Up PouchesTrash BagsInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil Method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Film Elongation at Break, MD 570 %
570 %
ASTM D882
Film Elongation at Break, TD 850 %
850 %
ASTM D882
Puncture Energy 3.16 J
2.33 ft-lb
ExxonMobil
Elmendorf Tear Strength, MD 3.15 g/micron
80.0 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 15.7 g/micron
400 g/mil
ASTM D1922
Dart Drop 3.94 g/micron
100 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 53.1 MPa
7700 psi
ASTM D882
Film Tensile Strength at Break, TD 35.2 MPa
5100 psi
ASTM D882
1% Secant Modulus, MD 193 MPa
28000 psi
ASTM D882
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
Peak Melting Temperature; ExxonMobil Method
Optical Properties Metric English Comments
Haze 15.3 %
15.3 %
ASTM D1003
Gloss 45 %
45 %
45°; ASTM D2457
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following: