Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1318CA Blown Film Resin  (discontinued **)
Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1518CA Tough Premium Film Resin  (discontinued **)
Exceed 1518CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
at 2% offset; ASTM D882
ExxonMobil LD 102.74 Thin Gauged Film Resin  (discontinued **)
LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin  (discontinued **)
Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Westlake LF1021 Butene Linear Low Density Polyethylene
Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
Westlake LF2040 Hexene Linear Low Density Polyethylene
Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength ..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin
Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, TD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..