Polymer Property : 1% Secant Modulus, TD = 223 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
1% Secant Modulus, TD 223 MPa
32300 psi
ASTM D882
ExxonMobil LL 1001x59 Blown Film Resin  (discontinued **)
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical