Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ CMU 236 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ CMU 236 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness/toughness balance is required.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/Toughness Good Dimensional StabilityLow EmissionsLow to No FoggingLow to No OdorMedium Impact Resistance Uses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Automotive Under the Hood Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527-2/50
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2/50
Elongation at Break 30 %
30 %
ISO 527-2/50
Elongation at Yield 3.0 %
3.0 %
ISO 527-2/50
Tensile Modulus 2.42 GPa
351 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.357 J/cm²

@Temperature 0.000 °C
1.70 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.672 J/cm²

@Temperature 22.8 °C
3.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
ISO 75-2/A