Polymer Property : Charpy Impact, Notched = 3.20 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.672 J/cm²

@Temperature 22.8 °C
3.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CMU 236 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness/toughness balance is required.Availa..
Charpy Impact, Notched 0.672 J/cm²

@Temperature -5.00 °C
3.20 ft-lb/in²

@Temperature 23.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNU 013 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South..