ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties along with excellent drawability make this a very versatile packaging film resin. It is available with blown film additive formulations with or without slip and antiblock. A heavily stabilized formulation for cast film processing is also available.Applications: Stretch wrap; Stretch film; Frozen food packaging; Ice bags; Shipping sacks; Premium trash bags. Data for film properties below based on 0.6 mil film.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
Exxon Method
Thickness 15.2 microns
0.600 mil
Melt Flow 1.0 g/10 min
1.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.1 MPa
1460 psi
ASTM D882
Film Tensile Strength at Yield, TD 8.50 MPa
1230 psi
ASTM D882
Film Elongation at Break, MD 530 %
530 %
ASTM D882
Film Elongation at Break, TD 710 %
710 %
ASTM D882
Secant Modulus, MD 0.193 GPa
28.0 ksi
ASTM D882
Secant Modulus, TD 0.221 GPa
32.1 ksi
ASTM D882
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
Elmendorf Tear Strength TD 500 g
500 g
ASTM D1922
Elmendorf Tear Strength, MD 11.1 g/micron
283 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 32.8 g/micron
833 g/mil
ASTM D1922
Dart Drop 7.20 g/micron
183 g/mil
F50; ASTM D1709
Dart Drop Test 110 g
0.243 lb
F50; ASTM D-1709
Film Tensile Strength at Break, MD 57.8 MPa
8380 psi
ASTM D882
Film Tensile Strength at Break, TD 41.9 MPa
6080 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
Exxon Method
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 51 %
51 %
45°, ASTM D-2457
Copyright © lookpolymers.com All Rights Reserved