Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Dart Drop Test | >= 110 g | >= 0.243 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | >= 110 g | >= 0.243 lb | ASTM D1709 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Dart Drop Test | 110 g | 0.243 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Dart Drop Test | 110 g | 0.243 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Dart Drop Test | 110 g | 0.243 lb | F<sub>50</sub>, Estimated from TEDD value of 0.3 ft-lbs. For standard dart and 26" drop height.; ASTM D1709 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Dart Drop Test | 110 g | 0.243 lb | Cast; ASTM D1709, F<sub>50</sub> |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Dart Drop Test | 110 g | 0.243 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Dart Drop Test | 110 g | 0.243 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA952094 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709 |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Dart Drop Test | 110 g | 0.243 lb | Cast; ASTM D1709, F<sub>50</sub> |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709 |
Westlake EF1807 Low Density Polyethylene Westlake Polyethylene EF1807 is a low density formulation suggested for film applications that require toughness.Application/UsesShrink filmFrozen food packagingFDA: This material complies with FDA .. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709A |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709A |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709A |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM D1709A |
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Dart Drop Test | 110 g | 0.243 lb | Film; 50.8 microns; ASTM D1709A |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |
|||
Dart Drop Test | 110 g | 0.243 lb | g/F50; ASTM D1709 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Dart Drop Test | 110 g | 0.243 lb | ASTM-D1709 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
Dart Drop Test | 110 g | 0.243 lb | g/F50; ASTM D1709 |
Braskem LH218 Cast Film Extrusion Linear Low Density Polyethylene Description: LH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability... |