ExxonMobil Solvesso™ Aromatic 200 ND Aromatic Fluid

Category Fluid
Manufacturer Exxon Chemical
Trade Name Solvesso™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Solvesso™ Aromatic 200 ND Aromatic Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appearance: Transparent-Slight Yellow LiquidAvailability: North AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.993 g/cc

@Temperature 15.6 °C
0.0359 lb/in³

@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 3.46 cSt
3.46 cSt
ASTM D445
Vapor Pressure <= 0.000133 bar

@Temperature 20.0 °C
<= 0.100 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 238 °C
460 °F
Initial; ASTM D86
Flash Point 113 °C
235 °F
ASTM D56
Descriptive Properties Value Comments
Aniline Point 57°F
Mixed, Method E, ASTM D611
Aromatic Content >99%
FIA, ASTM D1319
Dry Point 235°F
ASTM D86