Polymer Property : Elmendorf Tear Strength MD = 170 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene
ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil LD 334.57 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil LD 334.82 Clear, High Impact Film Resin
LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin
Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America..
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
Dow DOWLEX™ 2025G Linear Low Density Polyethylene
DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow
Elmendorf Tear Strength MD 170 g
170 g
ASTM D1922
ExxonMobil Exceed™ 2718CB Premium Cast Film Resin
Exceed 2718CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 2718CB resin have outstanding tensile properties and impact and puncture toughness..