ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:CompoundingHot Melt AdhesivesMaster Base ResinInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ExxonMobil Method
Vinyl Acetate Content 27.6 %
27.6 %
ExxonMobil Method
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
15s; ASTM D2240
Hardness, Shore D 19
19
15s; ASTM D2240
Tensile Strength at Break 4.83 MPa
700 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0186 GPa
2.70 ksi
1% secant; ASTM D790
Impact Test 14.9 J

@Temperature 23.0 °C
11.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
25.8 J

@Temperature -40.0 °C
19.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 66.1 °C
151 °F
Peak Melting Temperature; ExxonMobil Method