Physical Properties Metric English Comments
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1277A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1486A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1563 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1775D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1870-CR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1881E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Monprene® MP-2302 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer
Notes: Clear Features: High Flow; High Coefficient of FrictionInformation Provided by Teknor Apex
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Monprene® MP-2790 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2830C CLR Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
25.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB1732 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: Good UV Resistance Uses: Film Forms: Pellets Processing Method: Blow Mo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 2581B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1424A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1446G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1686D Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1686D1 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 25.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 150 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin
Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin
Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2830 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 25.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
25.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2830M UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..