Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 151 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 66.0 °C
151 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Melting Point 66.0 - 70.0 °C
151 - 158 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® 550 Thermoplastic Polyurethane
Pearlbondâ„¢ 550 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level...
Melting Point 66.0 - 70.0 °C
151 - 158 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® D170 Thermoplastic Polyurethane
Pearlbond® D170 is a TPU grade designed for use with Heat Sealable Fabrics. This grade is to be applied in thermo bonding (heat-sealing) processes, through which the adhesive is laid on a series..
Melting Point 66.0 °C
151 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® 741 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melting Point 66.0 °C
151 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res..
Melting Point 66.0 °C
151 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Melting Point 66.1 °C
151 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin
Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl..
Melting Point 66.1 °C
151 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin
Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl..
Melting Point 66.0 °C
151 °F
ASTM D3418, ISO 3146
DuPont™ Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer
DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to dete..
Melting Point 66.0 °C
151 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Surlyn® 8528 Sodium Ionomer
Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi..
Melting Point 66.0 °C
151 °F
DSC
Arkema Group LOTRYL® 35 BA 40 Copolymer Ethylene - Butyl Acrylate
LOTRYL® 35 BA 40 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 40 is particularly r..
Copyright © lookpolymers.com All Rights Reserved