Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 0.930 GPa | >= 135 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4340R (EP2Z29G) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | 880 min.; ASTM D790 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | At 1 mm/min; ISO 178 |
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen .. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
Ashley Polymers Ashlene® TD925H Nylon 12 A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption, with UV and he.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8761 HDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flowUses: Recreational products, Industrial components, RV tanks |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM-D790 |
Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa.. |
|||
Flexural Modulus | 0.930 GPa | 135 ksi | ASTM D790 |
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formula.. |