Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 203 J @Thickness 6.35 mm, Temperature -40.0 °C |
150 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
Impact Strength; Max Force; ARM |
ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formula.. |
|||
Impact Test | 203 J @Thickness 6.35 mm, Temperature -40.0 °C |
150 ft-lb @Thickness 0.250 in, Temperature -40.0 °F |
Impact Strength; Max Force; ARM |
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8760 is fully formula.. |