Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.210 - 0.250 g/cc
0.00759 - 0.00903 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 50 - 60
50 - 60
ASTM D 2240
Tensile Strength 0.800 MPa
116 psi
ASTM D 412
Elongation at Break >= 200 %
>= 200 %
ASTM D 412
Compressive Yield Strength 0.0650 MPa

@Strain 25.0 %
9.43 psi

@Strain 25.0 %
ASTM 1056/85
0.155 MPa

@Strain 50.0 %
22.5 psi

@Strain 50.0 %
ASTM 1056/85
Tear Strength 1.25 kN/m
7.13 pli
ASTM D 624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Vulcanization Peroxide