Unitika M1030E PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Unitika
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika M1030E PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nano composite nylonInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.20 mm
0.0080 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Thickness 3.20 mm
0.010 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 78.0 MPa
11300 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: