Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.25 kN/m | 7.13 pli | ASTM D 624 |
Eurofoam Porocell POR 446 NDN NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |