Polymer Property : Tear Strength = 7.13 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.25 kN/m
7.13 pli
ASTM D 624
Eurofoam Porocell POR 446 NDN NR-SBR Foam
Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.