Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength 49.6 MPa
7200 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
1.2 %
1.2 %
Flexural Strain; ASTM D790
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 92.4 MPa
13400 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Compressive Strength 193 MPa
28000 psi
10% Deformation; ASTM D695
Compressive Modulus 3.65 GPa
530 ksi
ASTM D695
Izod Impact, Notched 0.614 J/cm
1.15 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
ASTM D257
Descriptive Properties Value Comments
Color Black