Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 92.6 MPa | 13400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Strength | 92.39 MPa | 13400 psi | |
Abatron AboCast 8-11/Abocure 8-11 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 100 g (3.5 oz.): 93 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhe.. |
|||
Flexural Strength | 92.2 MPa | 13400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 92.2 MPa | 13400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 92.2 MPa | 13400 psi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® LX 2.0 Polyamide Composite Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability .. |
|||
Flexural Strength | 92.4 MPa @Temperature 22.8 °C |
13400 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger NORYL® Polyphenylene oxide (PPO) NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | ASTM D790 |
Aremco Aremco-Bond™ 2200 High Performance Epoxide Glass Fiber- and Kevlar-Reinforced, Epoxy-Novolac; High Strength, Excellent Abrasion and Corrosion Resistance |
|||
Flexural Strength | 92.4 MPa | 13400 psi | |
Abatron AboCast 8103-13 One-Component Epoxy AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested.. |
|||
Flexural Strength | 92.4 MPa | 13400 psi | for Epoxy Coating |
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Flexural Strength | 92.5 MPa | 13400 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |