Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D-638 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D-638 |
Plaskolite Optix® CP - 927 GHF High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D-638 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Formosa Plastics Formolon® AW02 Homopolymer/Compound Homopolymer/Compound Formolon (AW02) is a NSF approved medium molecular weight dry blend PVC compound. This compound has been engineered primarily for rigid extrusion applications. The exceptional .. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Formosa Plastics Formolon® AW04 Homopolymer/Compound Homopolymer/Compound Formolon (AW04) is a NSF approved medium molecular weight dry blend PVC compound. This compound has been engineered primarily for rigid extrusion applications. The exceptional .. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D638 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Tensile Strength | 49.6 - 63.4 MPa | 7200 - 9200 psi | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Tensile Strength | 49.6 - 63.4 MPa | 7200 - 9200 psi | |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Tensile Strength | 49.6 MPa | 7200 psi | ASTM D-638 |
Plaskolite West Optix® CP - 927 GHF High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |