Polymer Property : Izod Impact, Notched = 0.614 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.614 J/cm
1.15 ft-lb/in
ASTM D256
Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber
PET – Flame Retardant 30% Short Glass Fiber Reinforced. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM s..
Izod Impact, Notched 0.614 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.15 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.614 J/cm
1.15 ft-lb/in
ASTM D256
Ensinger Tecatron® XP-87 Compression Molded PPS Compound, 20% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Izod Impact, Notched 0.614 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.15 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedChemically CoupledInformation provided by PolyOne Corporation.