Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8088BL can be overmolded to polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Yield 11.76 MPa
1705 psi
ASTM D412
Elongation at Break 549 %
549 %
ASTM D412
100% Modulus 0.008150 GPa
1.182 ksi
ASTM D412
Compression Set 27 %

@Time 79200 sec
27 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature 79.0 °C
174 °F
Rear Barrel Temperature 177 - 193 °C
350 - 380 °F
Front Barrel Temperature 182 - 199 °C
360 - 390 °F
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi