Mechanical Properties Metric English Comments
100% Modulus 0.008150 GPa
1.182 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer
Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui..