Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 2850PE can be overmolded and coextruded with polyethylene.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
ASTM D2240
Tensile Strength 6.41 MPa
930 psi
ASTM D412
Elongation at Break 626 %
626 %
ASTM D412
100% Modulus 0.00173 GPa
0.251 ksi
ASTM D412
Compression Set 16 %

@Temperature 20.0 °C,
Time 79200 sec
16 %

@Temperature 68.0 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature <= 79.4 °C
<= 175 °F
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Front Barrel Temperature 182 - 188 °C
360 - 370 °F
Nozzle Temperature 193 - 204 °C
380 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa
100 - 200 psi
Descriptive Properties Value Comments
Injection Rate Fast
Users viewing this material also viewed the following: