Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00173 GPa | 0.251 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for.. |