Material Notes:
Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades of Eastman Tritan. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan LX150HF was developed for the cosmetic, fragrance, and personal care markets. Tritan LX150HF can easily be converted into articles for application in consumer and personal markets by injection molding, extrusion blow molding, and injection blow molding.Application/UsesCosmetics hot-fill packagingCosmetics/personal care packagingFragrance packagingKey AttributesEase of processingexcellent clarityFast drying timesGood chemical resistanceGood heat resistanceImproved flowabilityOutstanding impact resistanceQuick cycle timesReported typical properties are preliminary. Information was provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength at Break 52.0 MPa
7540 psi
ASTM D638
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 1.575 GPa
228.4 ksi
ASTM D638
Flexural Yield Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 1.575 GPa
228.4 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Temperature -40.0 °C
2.06 ft-lb/in

@Temperature -40.0 °F
ASTM D256
8.60 J/cm

@Temperature 23.0 °C
16.1 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 53.0 J

@Temperature 23.0 °C
39.1 ft-lb

@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
57.0 J

@Temperature -40.0 °C
42.0 ft-lb

@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 260 - 282 °C
500 - 540 °F
Mold Temperature 38.0 - 66.0 °C
100 - 151 °F
Drying Temperature 88.0 °C
190 °F
Dry Time 4 - 6 hour
4 - 6 hour