Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 49.0 - 66.0 °C | 120 - 151 °F | |
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | Injection Molding |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | Injection Molding |
Ineos ABS Lustran® 750 ABS, Molding Grade Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl.. |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | Injection Molding |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Mold Temperature | 43.0 - 66.0 °C | 109 - 151 °F | Injection Molding |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX810 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceOutstanding impact re.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan MX811 Copolyester Applications:Blood TherapyDialyzer HousingsIV ComponentsKey Attributes:Ease of processingExcellent clarityExcellent hydrolytic stabilityFast drying timesGood chemical resistanceGood heat resistanceO.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX1000 Copolyester Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX1001 Copolyester Eastman Tritan TX1001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX1001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX1500HF Copolyester Eastman Tritan TX1500HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1500HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1000. Other outstanding features.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX2000 Copolyester Eastman Tritan TX2000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistanc.. |
|||
Mold Temperature | 38.0 - 66.0 °C | 100 - 151 °F | |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |