Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP RL008 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RL008 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RL008 is a compound based on PA 66 containing PTFE. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
5 mm/min; ISO 527
Elongation at Break 8.2 %
8.2 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 67.0 MPa
9720 psi
2 mm/min; ISO 178
Flexural Modulus 2.00 GPa
290 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 207 °C
405 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af