Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 57.0 J @Temperature -40.0 °C |
42.0 ft-lb @Temperature -40.0 °F |
Energy @ Max. Load; ASTM D3763 |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |