Material Notes:
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high current interconnects, pin grids, welding wire, or other elevated temperature applications.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 56 - 62
56 - 62
Thickness > 0.020 Inch
Tensile Strength, Ultimate 324 - 386 MPa
47000 - 56000 psi
Tensile Strength, Yield 317 - 372 MPa
46000 - 54000 psi
0.2% offset
Elongation at Break 2.0 - 9.0 %
2.0 - 9.0 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 17.6 µm/m-°C

@Temperature 20.0 - 300 °C
9.80 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 359.7 W/m-K
2496 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 99.9 %
99.9 %
Zirconium, Zr 0.10 %
0.10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000187 ohm-cm
0.00000187 ohm-cm
Annealed