Polymer Property : Tensile Strength, Yield = 46000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 317 MPa

@Strain 0.200 %
46000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, mill annealed
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 317 MPa

@Strain 0.200 %
46000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 317 MPa

@Strain 0.200 %
46000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 110 EPT COPPER, Extra Hard
Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of ..
Tensile Strength, Yield 317 - 372 MPa
46000 - 54000 psi
0.2% offset
Eagle Brass 151 ZHC® COPPER, 3/4 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 101 OFE COPPER (Certified), Extra Hard
Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information..
Tensile Strength, Yield 317 - 379 MPa
46000 - 55000 psi
0.2% offset
Eagle Brass 102 OF COPPER (Non-Certified), Extra Hard
Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an..
Tensile Strength, Yield 317 - 345 MPa
46000 - 50000 psi
Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy
Finished product available in rods.Chicago Extruded Metal temper code: H02This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Tensile Strength, Yield 317 MPa

@Strain 0.200 %
46000 psi

@Strain 0.200 %
Carpenter 20Cb-3® Stainless Steel, Strip, Annealed at 1750°F (955°C) then Water Quenched
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Yield 317 MPa

@Strain 0.200 %
46000 psi

@Strain 0.200 %
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..