Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 296 - 372 MPa | 42900 - 54000 psi | With 0% cold work |
OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper GlidCop® AL-25 is copper that is dispersion strengthened with 0.5 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Tensile Strength, Yield | 317 - 372 MPa | 46000 - 54000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, 3/4 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 296 - 372 MPa | 43000 - 54000 psi | 0.2% offset |
Eagle Brass 230 Red Brass, 1/2 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Strength, Yield | 138 - 372 MPa | 20000 - 54000 psi | 0.2% offset |
Eagle Brass 425 Tin Brass 2%, 1/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Yield | 345 - 372 MPa @Strain 0.200 %, Thickness 1.02 mm |
50000 - 54000 psi @Strain 0.200 %, Thickness 0.0402 in |
|
AK Steel 11 Cr-Cb™ Ferritic Stainless steel AK Steel 11 Cr-Cb™ has increased silicon levels and is dual stabilized with titanium and columbium. Designed for use in automotive exhaust tubing and other high-temperature applications, this is a.. |