Material Notes:
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparencyLow melting point (200°C) Application examples: Grilon CR 9 is suitable for the manufacture of both blown and cast coextruded film. Grilon CR 9 is suitable for the following applications: Flexible packaging, e.g. “Cook in ham”, consumer packaging of meat, cheese, smoked ham, fish, sausage, poultry and peanuts as well as many other foodstuffs.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 55.0 cc/m²/day
3.54 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
75.0 cc/m²/day
4.83 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 200 cc-mm/m²-24hr-atm
508 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
350 cc-mm/m²-24hr-atm
889 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 120 g/10 min
120 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Yield, TD 30.0 MPa
4350 psi
ISO 527-3
Film Elongation at Break, MD 800 %
800 %
ISO 527-3
Film Elongation at Break, TD 900 %
900 %
ISO 527-3
Film Elongation at Yield, MD 10 %
10 %
ISO 527-3
Film Elongation at Yield, TD 10 %
10 %
ISO 527-3
Tensile Modulus 0.550 GPa
79.8 ksi
conditioned; ISO 527-1/-2
Tear Strength 65.0 kN/m
371 pli
Trouser Tear resistance MD; ISO 6383-1
65.0 kN/m
371 pli
Trouser Tear resistance TD; ISO 6383-1
Elmendorf Tear Strength MD 2040 g
2040 g
ISO 6383-2
Elmendorf Tear Strength TD 2040 g
2040 g
ISO 6383-2
Film Tensile Strength at Break, MD 80.0 MPa
11600 psi
ISO 527-3
Film Tensile Strength at Break, TD 75.0 MPa
10900 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Gloss 130 %
130 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
FDA
Form Granules
Gelboflextest [holes/m²], EMS 800
Packaging Oriented film
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
Flexible
High viscosity
Special Characteristics Transparent