Carbon Dioxide Transmission 350 cc-mm/m²-24hr-atm
889 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® CR 9 HV PA*
Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr..
Carbon Dioxide Transmission 350 cc-mm/m²-24hr-atm
889 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® CR 9 PA*
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH..